Polymer Property : Hot Ball Pressure Test = 100 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East)
CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide ..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS
PC+ ABS General Purpose Non-FR
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS
PC+ ABS Automotive applications
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific)
PC+ ABS Automotive applications
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East)
PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging.
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This ..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East)
XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific)
DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r..
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East)
NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815.
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East)
LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications.
Hot Ball Pressure Test >= 100 °C
>= 212 °F
BS 3456, IEC 335
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS
Hot Ball Pressure Test >= 100 °C
>= 212 °F
BS 3456, IEC 335
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene
Hot Ball Pressure Test >= 100 °C
>= 212 °F
BS 3456, IEC 335
EPICHEM Epiryl PPO V0 Polyphenylene oxide
Characteristics: self-extinguishing V0 at 1,6 mm
Hot Ball Pressure Test >= 100 °C
>= 212 °F
BS 3456, IEC 335
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS
Characteristics: Thermic resistant
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Hot Ball Pressure Test <= 100 °C
<= 212 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha..