Polymer Property : Hot Ball Pressure Test = 130 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 130 °C
<= 266 °F
IEC 60695-10-2
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East)
XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab..
Hot Ball Pressure Test <= 130 °C
<= 266 °F
IEC 60695-10-2
SABIC Innovative Plastics Noryl PX1115 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX1115 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL PX1115 is V1 at 1.2 mm according UL94 and halogen free according VDE/DIN 472 part 815.Th..