Thermal Properties Metric English Comments
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® 3158 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® ET2613 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi..
Hot Ball Pressure Test 138 °C
280 °F
IEC 60695-10-2
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..