Polymer Property : Hot Ball Pressure Test = 88.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test 88.0 °C
190 °F
IEC 60335-1
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..