Hot Ball Pressure Test 96.0 °C

@Thickness 2.00 mm
205 °F

@Thickness 0.0787 in
IE/CEN 60335-1
Sax Polymers SAXLAC 120U Acrylonitrile Butadiene Styrene
Saxalac 120U is an UV protected easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested..