Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 1.23 µm/m-°C @Temperature 23.0 - 60.0 °C |
0.683 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |
|||
CTE, linear, Parallel to Flow | 1.23 µm/m-°C @Temperature -40.0 - 40.0 °C |
0.683 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |