Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 143 µm/m-°C @Temperature -40.0 - 40.0 °C |
79.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 143 µm/m-°C @Temperature -40.0 - 40.0 °C |
79.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 143 µm/m-°C @Temperature -40.0 - 40.0 °C |
79.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |