Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 30.0 - 300 °C |
83.3 µin/in-°F @Temperature 86.0 - 572 °F |
|
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 55.0 - 100 °C |
83.3 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 55.0 - 100 °C |
83.3 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 55.0 - 160 °C |
83.3 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 55.0 - 160 °C |
83.3 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 23.0 - 55.0 °C |
83.3 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Parallel to Flow | 150 µm/m-°C @Temperature 23.0 - 55.0 °C |
83.3 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |