Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 100 - 200 °C
8.89 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -20.0 - 150 °C
8.89 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2310F PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2310F PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 150 °C
8.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 100 - 200 °C
8.89 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -50.0 - 90.0 °C
8.89 µin/in-°F

@Temperature -58.0 - 194 °F
2
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 100 - 200 °C
8.89 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.89 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -20.0 - 150 °C
8.89 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2310 PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2310 PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -20.0 - 150 °C
8.89 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -20.0 - 150 °C
8.89 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.89 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.89 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DEF42 PC
LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
8.89 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DEF42 PC
LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 100 - 200 °C
8.89 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
CTE, linear, Parallel to Flow 16.0 µm/m-°C

@Temperature 0.000 - 90.0 °C
8.89 µin/in-°F

@Temperature 32.0 - 194 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..