Polymer Property : CTE, linear, Parallel to Flow = 2.22 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.22 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK
LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber.
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.22 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific)
LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber.
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
2.22 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature 140 - 180 °C
2.22 µin/in-°F

@Temperature 284 - 356 °F
ISO 11359-1/-2
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..