Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 29.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 53.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific)
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.
CTE, linear, Parallel to Flow 53.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS
LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral.
CTE, linear, Parallel to Flow 53.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved