Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL N1150 PPE+PS
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
CTE, linear, Parallel to Flow 54.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL N1150 PPE+PS
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
CTE, linear, Parallel to Flow 54.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
CTE, linear, Parallel to Flow 54.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
CTE, linear, Parallel to Flow 54.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
CTE, linear, Parallel to Flow 54.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
30.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..