Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer
High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer
High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific)
High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific)
High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East)
High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East)
High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific)
Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel..
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect..
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10
LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti..