Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KFL25 Acetal Copolymer
LNP LUBRICOMP* KFL25 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 82.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66
LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant.