Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008S PP
LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific)
LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East)
LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized.
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008SU PP
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008SU PP (Asia Pacific)
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East)
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized.
CTE, linear, Parallel to Flow 46.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East)
LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized.