Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG8000SR ABS
This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG8000SR ABS
This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FE8000S PPE+PS
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FE8000S PPE+PS
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
CTE, linear, Parallel to Flow 87.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..