Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 6.00 µm/m-°C @Temperature >=143 °C |
3.33 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
CTE, linear, Parallel to Flow | 6.00 µm/m-°C @Temperature <=143 °C |
3.33 µin/in-°F @Temperature <=289 °F |
Below Tg; ASTM D696 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
CTE, linear, Parallel to Flow | 6.00 µm/m-°C @Temperature >=143 °C |
3.33 µin/in-°F @Temperature >=289 °F |
Above Tg; ASTM D696 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |