Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Asia Pacific) Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS7R PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS7R PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPS7R PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific) LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific) LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Asia Pacific) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |