Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 66.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm