Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 124R PC UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2R PC Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® VR2520 PC General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HF1140 PC Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP3REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 365 PC+PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |