CTE, linear, Parallel to Flow 68.7 µm/m-°C

@Temperature -40.0 - 95.0 °C
38.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM141R PC
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
CTE, linear, Parallel to Flow 68.7 µm/m-°C

@Temperature -40.0 - 95.0 °C
38.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
CTE, linear, Parallel to Flow 68.7 µm/m-°C

@Temperature -40.0 - 95.0 °C
38.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..