Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY FXW749SK ASA
Sparkle VisualFx ASA Resin - Weatherable
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature 23.0 - 55.0 °C
57.8 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER
Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature 23.0 - 55.0 °C
57.8 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature 23.0 - 55.0 °C
57.8 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature 23.0 - 55.0 °C
57.8 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature 23.0 - 55.0 °C
57.8 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region.