Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 196 µm/m-°C

@Temperature -40.0 - 40.0 °C
109 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
CTE, linear, Transverse to Flow 196 µm/m-°C

@Temperature -40.0 - 40.0 °C
109 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific)
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia..
CTE, linear, Transverse to Flow 196 µm/m-°C

@Temperature 23.0 - 150 °C
109 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)