Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect.. |
|||
CTE, linear, Transverse to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
CTE, linear, Transverse to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific) LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 LNP* THERMOCOMP* IC006 is a compound based on Nylon 6/12 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 (Asia Pacific) LNP* Thermocomp* IC006 is a compound based on Nylon 6/12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |