Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 19.5 µm/m-°C @Thickness 2.00 mm, Temperature 125 °C |
10.8 µin/in-°F @Thickness 0.0787 in, Temperature 257 °F |
|
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
CTE, linear, Transverse to Flow | 19.5 - 25.0 µm/m-°C @Temperature 75.0 - 175 °C |
10.8 - 13.9 µin/in-°F @Temperature 167 - 347 °F |
Average value: 22.3 µm/m-°C Grade Count:1 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
CTE, linear, Transverse to Flow | 19.5 - 25.0 µm/m-°C @Thickness 2.00 - 4.00 mm |
10.8 - 13.9 µin/in-°F @Thickness 0.0787 - 0.157 in |
Average value: 22.3 µm/m-°C Grade Count:1 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |