Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 190 µm/m-°C

@Temperature 23.0 - 55.0 °C
106 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
CTE, linear, Transverse to Flow 190 µm/m-°C

@Temperature 55.0 - 120 °C
106 µin/in-°F

@Temperature 131 - 248 °F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..