Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
CTE, linear, Transverse to Flow | 53.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare. |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare. |
|||
CTE, linear, Transverse to Flow | 53.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
CTE, linear, Transverse to Flow | 53.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release |
|||
CTE, linear, Transverse to Flow | 53.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific) LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |