Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 31.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound  (discontinued **)
Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun..
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly
LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp DF0069E PC
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific)
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK
LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber.
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific)
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit..
Copyright © lookpolymers.com All Rights Reserved