Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 31.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Asia Pacific)
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Asia Pacific)
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific)
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
31.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific)
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
31.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 100 - 150 °C
31.1 µin/in-°F

@Temperature 212 - 302 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber
Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 150 °C
31.1 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 150 °C
31.1 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific)
High flow Ultem blends for thin wall application
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 150 °C
31.1 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East)
High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 50.0 - 100 °C
31.1 µin/in-°F

@Temperature 122 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
CTE, linear, Transverse to Flow 55.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6
LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6
LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ASTM E 228
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 50.0 - 100 °C
31.1 µin/in-°F

@Temperature 122 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, ..
Copyright © lookpolymers.com All Rights Reserved