Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Transverse to Flow | 34.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |