CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12
LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific)
LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS
LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant.