Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 70.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 70.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |