Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66
LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific)
LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific)
LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
CTE, linear, Transverse to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
CTE, linear, Transverse to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East)
Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating ..