Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 51.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DDF029 PC
LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant.