Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 94.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
52.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..