Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific)
Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific)
Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.This data was suppli..
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan..
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 23.0 °C
29.4 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 200 °C
29.4 µin/in-°F

@Temperature 392 °F
ASTM D696
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66  (Unverified Data**)
Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ASTM E 831
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66  (Unverified Data**)
Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ASTM E 831
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 150 °C
29.4 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 23.0 - 150 °C
29.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 150 °C
29.4 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 23.0 - 150 °C
29.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 150 °C
29.4 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 23.0 - 150 °C
29.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific)
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 200 - 300 °C
29.4 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
Ensinger TECASINT 1011 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00CES PA 66
LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific)
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RX06424 PA 66
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural