CTE, linear, Transverse to Flow 99.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
55.0 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 99.0 µm/m-°C

@Temperature 25.6 - 93.3 °C
55.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..