Polymer Property : CTE, linear, Transverse to Flow = 64.5 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 64.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer
High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors. US ..
CTE, linear, Transverse to Flow 64.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer
High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors. US ..