Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 65.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly
LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly
LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON MS000IL PP
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c..
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON MS000IL PP
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c..