CTE, linear, Transverse to Flow 118 µm/m-°C

@Temperature 23.0 - 55.0 °C
65.6 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66  (Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 118 µm/m-°C

@Temperature 23.0 - 55.0 °C
65.6 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66  (Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers