Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 55.0 - 160 °C |
69.4 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 55.0 - 160 °C |
69.4 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 55.0 - 160 °C |
69.4 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 55.0 - 160 °C |
69.4 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature 23.0 - 60.0 °C |
69.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 125 µm/m-°C @Temperature -40.0 - 40.0 °C |
69.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |