Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 101 °C | 214 °F | ISO 75B |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
Heat Distortion Temperature | 101 °C | 214 °F | ISO 75B |
Lucite International Diakon® CLH952LX Acrylic Polymer Information provided by Lucite International |