Polymer Property : Heat Distortion Temperature = 253 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 253 °C
487 °F
ASTM D648
Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..