Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 123 °C | 253 °F | ISO 75-2 |
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |