Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 131 °C | 268 °F | ASTM D648 |
Kotec Carbotex K-20 Polycarbonate, General Purpose Features: Standard, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformation .. |
|||
Heat Distortion Temperature | 131 °C | 268 °F | ASTM D648 |
Kotec Carbotex K-20MRA Polycarbonate, General Purpose, Mold Release Grade Features: Mold Release, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformat.. |
|||
Heat Distortion Temperature | 131 °C | 268 °F | ASTM D648 |
Kotec Carbotex K-20UV Polycarbonate, General Purpose, UV Stability Grade Features: UV Stability, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Heat Distortion Temperature | 131 °C | 268 °F | ASTM D648 |
Kotec Carbotex K-20UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household app.. |
|||
Heat Distortion Temperature | 131 °C | 268 °F | ASTM D648 |
Kotec Carbotex KV-20FD Polycarbonate, Food Grade Features: Food contact, High flow, Mold release, TransparentApplications: Household appliance, Kitchenware, Food packaging/containersInformation provided by Kotec Corporation |