Thermal Properties Metric English Comments
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Kotec Carbotex K-30FRT12 Polycarbonate, Flame Retardant
Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo..
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Kotec Carbotex K-40 Polycarbonate, General Purpose
Features: Standard, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications, Le..
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Kotec Carbotex K-40MRA Polycarbonate, General Purpose, Mold Release Grade
Features: Mold release, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications..
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Kotec Carbotex K-40UV Polycarbonate, General Purpose, UV Stability Grade
Features: UV stability, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications..
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Kotec Carbotex K-40UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade
Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household application..
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Kotec Carbotex KFR-30T12 Polycarbonate, Flame Retardant
Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo..
Heat Distortion Temperature 133 °C
271 °F
ISO 75-2
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..