Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 143 °C | 289 °F | ASTM D648 |
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Heat Distortion Temperature | 143 °C | 289 °F | ASTM D648 |
Kotec Carbotex KGN-15MRA Polycarbonate, Flame Retardant, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Heat Distortion Temperature | 143 °C | 289 °F | DIN 53 461, ISO R 75 process A |
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK) TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al.. |