Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 197 °C | 387 °F | ISO 75-2 |
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Heat Distortion Temperature | 197 °C | 387 °F | ISO 75-2 |
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |