Polymer Property : Heat Distortion Temperature = 39.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 39.0 °C
102 °F
ISO 75
Iran Petrochemical (PCC) 1922T Low Density Polyethylene
LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co..