Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Heat Distortion Temperature = 40.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 40.0 °C
104 °F
HDT B; ISO 75
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Heat Distortion Temperature 40.0 °C
104 °F
3M Scotchkote™ SG 527 Epoxy Metal Repair
Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.P..